De meast brûkte graden binne | Gr5(Ti-6Al-4V), Gr23(Ti-6Al-4V ELI), Ti-6Al-7Nb |
Standert | ASTM F136, ISO 5832-3, ASTM F1295/ISO 5832-11 |
Diameter | 3-100mm |
Tolerânsje | h7, h8, h9 |
Oerflak | Gepolijst |
Rjochtheid | Binnen 1.5‰ |
Karakteristyk | Wy kinne jo oanpaste produkten mei hege prestaasjes dwaan |
Gemyske gearstallingen | ||||||||
Klasse | Ti | Al | V | Fe, maks | C, maks | N, maks | H, maks | O, maks |
Ti-6Al-4V ELI | Bal | 5.5~6.5 | 3.5~4.5 | 0.25 | 0.08 | 0.05 | 0.012 | 0.13 |
Graad 5 (Ti-6Al-4V) | Bal | 5.5~6.75 | 3.5~4.5 | 0.3 | 0.08 | 0.05 | 0.015 | 0.2 |
Ti-6Al-7Nb | Bal | 5.5~6.5 | Nb: 6.5~7.5 | 0.25 | 0.08 | 0.05 | 0.009 | 0.2 |
Mechanyske eigenskippen | |||||
Klasse | Betingst | Treksterkte (Rm/Mpa) ≥ | Opbringststerkte (Rp0.2/Mpa) ≥ | Ferlinging (A%) ≥ | Reduksje fan oerflak (Z%) ≥ |
Ti-6Al-4V ELI | M | 860 | 795 | 10 | 25 |
Graad 5 (Ti-6Al-4V) | M | 860 | 780 | 10 | / |
Ti-6Al-7Nb | M | 900 | 800 | 10 | 25 |
XINNUO ymportearre Dútske ALD Vacuum Oven om de titanium ingots sels te smelten sûnt 2016, 3 kear te smelten om te soargjen dat de gemyske gearstallingen evenredich binne, en it waarmtenûmer fan titanium ingots nei elk lettere produksjeproses te markearjen, it te printsjen op 'e definitive gepoleerde balken foar lettere tracking.
Mei elke partij guod testen wy de treksterkte mei ús spanningstester en nimme wy ek in stekproef mei nei it laboratoarium fan tredden, en leverje wy in mûnetestsertifikaat oan klanten.
100% ultrasone flater ûntdutsen, waarmtenûmer en produksjeproses binne traceerber, en XINNUO nimt de kwaliteit fan 'e guod as it earste wichtige ding tidens it heule produksjeproses, sil de net-kwalifisearre produkten net út 'e fabryk leverje litte, ferantwurdlik foar elke batch levere guod.